Tempering
At its Kıraç and Kırklareli facilities, Camglass applies full tempering and heat strengthening to flat glass. Processing capacity covers ceramic printed and enamelled glass as well as toughenable Low-E and Solar Low-E glass, including double-silver options.
Coated glass is processed in accordance with the glass manufacturer’s heat treatment conditions. Mechanical processing and surface applications are completed before tempering.
In line with the project specification, fully tempered glass undergoes heat soak testing in accordance with TS EN 14179. The test reduces the risk of spontaneous breakage caused by nickel sulphide.
Overview
Superior Strength
Approximately 5 times stronger than untreated glass.
Thermal Stress Resistance
Superior performance against impact and thermal stress.
Safe Breakage
Breaks into small, dice-sized fragments.
Related Products
Tempered Safety Glass
Heat-Strengthened Glass
Enamelled Tempered Glass
Screen Printing
Applications
Hotels & Hospitality
Façade Systems
Door Applications
Shopfront Glazing
Glass Balustrade
Balustrades and Handrails
Technical Details
| Facility | Glass thickness | Maximum Size | Minimum Size |
|---|---|---|---|
Kırklareli | 5–19 mm | 6000 × 3300 mm | 300 × 300 mm |
Kıraç | 5–19 mm | 5000 × 2850 mm | 300 × 300 mm |
Kıraç | 4 mm | 2000 × 2850 mm | 300 × 300 mm |